How to Prevent Part-on-Part Damage in Vibratory Finishing How to Prevent Part-on-Part Damage in Vibratory Finishing Short answer: part-on-part damage is usually a contact-control problem. Protect the workpieces with enough media coverage, a suitable media size and shape, a stable load ratio and a machine motion that keeps parts separated. Confirm the change with before-and-after inspection instead...
How to Choose Media Size for Small Holes, Slots and Internal Cavities How to Choose Media Size for Small Holes, Slots and Internal Cavities Short answer: choose the smallest media that reaches the required feature and can still be separated reliably. A smaller chip may improve access, but it can also lodge in a hole, pass through a slot, slow separation or change the contact intensity. The correct...
How to Choose Media Size for Small Holes, Slots and Internal Cavities How to Choose Media Size for Small Holes, Slots and Internal Cavities Short answer: choose the smallest media that reaches the required feature and can still be separated reliably. A smaller chip may improve access, but it can also lodge in a hole, pass through a slot, slow separation or change the contact intensity. The correct...
How to Choose Media Size for Small Holes, Slots and Internal Cavities How to Choose Media Size for Small Holes, Slots and Internal Cavities Short answer: choose the smallest media that reaches the required feature and can still be separated reliably. A smaller chip may improve access, but it can also lodge in a hole, pass through a slot, slow separation or change the contact intensity. The correct...
How to Choose Media Size for Small Holes, Slots and Internal Cavities How to Choose Media Size for Small Holes, Slots and Internal Cavities Short answer: choose the smallest media that reaches the required feature and can still be separated reliably. A smaller chip may improve access, but it can also lodge in a hole, pass through a slot, slow separation or change the contact intensity. The correct...
Double-Deck Bamboo Tumbling Machine: Standard Operating Procedure, Control Guide & Finishing Recipes Model Series: SP-TB4 / SP-TB8 • Precision Dry Tumbling System • Official operation manual The SP-TB Series double-deck bamboo tumbling machine is a precision dry tumbling system designed for high-gloss finishing of premium eyewear frames (acetate, propionate), fine hardware, jewelry, and luxury...
Walnut Shell vs Corncob: How to Choose Dry Tumbling Media for Eyewear, Jewelry & Hardware Dry finishing media selection guide • Walnut shell & corncob • For dry tumbling, vibratory and centrifugal lines Dry organic media — crushed walnut shell and ground corncob — is the workhorse of dry tumbling and dry vibratory finishing. The two materials look similar in the bag, but they behave very d...
Centrifugal Disc vs Centrifugal Barrel Finishing: Which High-Energy Machine Fits Your Parts? High-energy mass finishing comparison • Centrifugal disc & centrifugal barrel • Machine selection guide When vibratory finishing is too slow or too gentle for the result you need, the next step up in intensity is a centrifugal disc or a centrifugal barrel machine. Both multiply the effective force betw...
Mass Finishing for 3D Printed Parts: Deburring and Polishing Additive Manufacturing Components Additive manufacturing post-processing • Deburring, smoothing & polishing • FDM, SLA/DLP, SLS & metal AM parts 3D printing turns out parts close to final shape, but almost never close to final surface. Support scars, layer lines, partially fused powder, and sharp edges stand between a fresh print...